인공타액 오염이 수종 상아질접착제와 상아질간의 결합에 미치는 영향
[STEP1]서지반출 형식 선택
파일형식
@
서지도구
SNS
기타
[STEP2]서지반출 정보 선택
  • 제목
  • URL
돌아가기
확인
취소
  • 인공타액 오염이 수종 상아질접착제와 상아질간의 결합에 미치는 영향
저자명
류미애,양규호,오원만,Ryu. Mee-Ae,Yang. Kyu-Ho,Oh. Won-Mann
간행물명
大韓齒科保存學會誌
권/호정보
1992년|17권 2호|pp.383-397 (15 pages)
발행정보
대한치과보존학회
파일정보
정기간행물|
PDF텍스트
주제분야
기타
이 논문은 한국과학기술정보연구원과 논문 연계를 통해 무료로 제공되는 원문입니다.
서지반출

기타언어초록

The purpose of this study was to evaluate the influence of artificial saliva contamination on bonding of several dentin adhesives to dentin. Sixty - three human molar teeth extracted within a month were used. Each tooth was sectioned longitudinally in a buccolingual direction to obtain 126 specimens. These specimens were randomly divided into three groups and were treated by Scotchbond 2, Gluma and All bond. Each group was subdivided into three subgroups; normal group not contaminated with artificial saliva, contaminated with artificial saliva and dried group, and contaminated with artificial saliva and washed and dried group. Enamel/dentin bonding agent(Dental Adhesive of Scotchbond 2) was applied and light cured on the treated dentin surfaces. Thereafter P - 50 were cured on them, and specimens were stored in $37^{circ}C$ artificial saliva for 24 hours before measuring shear bond strength. Shear bond strengths were determined using an universal testing machine with cross head speed 1mm/min and SEM examinations were conducted to evaluate the resin - dentin interface and degree of penetrating resin string into the dentinal tubules. The following results were obtained. 1. Normal groups not contaminated with artificial saliva showed greater shear bond strength than any other group contaminated with artificial saliva(P<0.01). 2. The shear bond strengths showed no significant difference between washed groups with distilled water and not washed groups after contamination with artificial saliva(P>0.05). 3. In normal groups, the shear bond strength of A group was significantly greater than in any other group(P<0.01). 4. In Sand G groups, fractures after shear bond strength tests occured adhesively on resintooth interface in all specimens. But in A groups, fracture of the normal group occured cohesively in dentin and fracture of the contaminated groups occured adhesively and cohesively. 5. On SEM examination, the number of resin strings penetrated into dentinal tubules were the greatest in normal groups, followed by, in descending order, washed groups and not washed groups after contamination with artificial saliva.