- SA508-3재의 제하컴플라이언스법과 하중비해석을 이용한 파괴저항곡선 평가
- ㆍ 저자명
- 임만배,차귀준,윤한기,안원기
- ㆍ 간행물명
- 韓國海洋工學會誌
- ㆍ 권/호정보
- 1998년|12권 1호|pp.65-75 (11 pages)
- ㆍ 발행정보
- 한국해양공학회
- ㆍ 파일정보
- 정기간행물| PDF텍스트
- ㆍ 주제분야
- 기타
The fracture resistance curve is one of most important and design techniques employed in nuclear pressure vessel structures. This study is to evaluate the J-R curve characteristics for the SA508C-3 by the unloading compliance method and load rato analysis. The effect of strain aging for the exponential correlation of the J-R curve in this metal are investigated at room temperature, 20$0^{circ}C$ and 30$0^{circ}C$. The load ratio analysis method can evaluate the J-R curve by using the simple tension load-displacement curve only without the repeat of the unloading and loading. Therefore, the analysis by the proposed load ratio method has a merit, in comparison with the unloading compliance method, which can measure the crack length without the precision measurement equipment.