- $CaSO_4:Tb$ TLD의 제작과 특성에 관한 연구
- A Study on Fabrication and Characteristics of $CaSO_4:Tb$ TLD
- ㆍ 저자명
- 박명환,Park. Myeong-Hwan
- ㆍ 간행물명
- 대한방사선기술학회지
- ㆍ 권/호정보
- 1999년|22권 1호|pp.55-60 (6 pages)
- ㆍ 발행정보
- 대한방사선과학회
- ㆍ 파일정보
- 정기간행물| PDF텍스트
- ㆍ 주제분야
- 기타
In this study, the highly sensitive $CaSO_4:Tb$ glass capsule type TLDs are fabricated and their trap parameters are determined. The optimum conditions of fabricating of $CaSO_4:Tb$ phosphor was obtained to be in impurity concentration of Tb 1.0 mol% and sintering of $600^{circ}C$, 2 hr. The glow curve of $CaSO_4:Tb$ consists of three glow peaks and these peaks are isolated by thermal bleaching method. Activation energy of the three glow peaks measured by the initial rise, the peak shape and the heating rate method are 0.70, 0.87, and 1.03 eV. The frequency factors are $1.76{ imes}10^9,;1.74{ imes}10^9$, and $9.77{ imes}10^8;s^{-1}$, and the kinetic orders are 1.12, 1.46, and 1.34, respectively. The isolated glow peaks are fitted by least square method and optimum temperature range of the main peak for radiation dosimetry is $230{sim}295^{circ}C$.