  • 황칠처리재의 도막 물성 및 내구성
저자명
조종수,김종인
간행물명
가구
권/호정보
2001년|12권 1호|pp.11-20 (10 pages)
발행정보
한국가구학회
파일정보
정기간행물|
PDF텍스트
주제분야
기타
이 논문은 한국과학기술정보연구원과 논문 연계를 통해 무료로 제공되는 원문입니다.
서지반출

기타언어초록

To investigate weathering and surface characteristics of coating film on lumbers coated with Hwangchil(varnish of Dendropanax morbifera), we carried out to investigate the resistance against discoloration, value of crack and surface characteristics of coating films on seven domestic lumbers and those of four introduced tropical lumbers. There was investigated to evaluate the properties of coating films by the varnish of Dendropanax morbifera. There was insignificant correlations between the hardness and moisture contents of each lumber treated by the varnish. There was no significant correlations between the thickness of coating film and the hardness, either. Although we investigated 11 wood species, we found only three species as resistance wood species against discoloration; Diospysos spp., Abies holophylla and Ulmus davidiana. The crack of coaing films was the largest on Zelkova serrata followed by Juglans sinensis, Cercidiphum japonicum, Tectona grands, Ulmus davidiana, Guibourtia tessmannii, Diospysos spp. and Dalbergia latifolia. However, there was no crack of coating films on the lumbers of Juniperus rigida, Prunus serrulata var. spontanea and Abies holophylla. The crack of coating film showed positive correlations with the thickness of coating film and hardness. The surface characteristics of the coating films evaluated on the basis of $R_{a}$ values indicated the lumbers of Ulmus davidiana($0.14{;}{mu}m$), Juniperus rigida($0.1 5{;}{mu}m$), Guibourtia tessmannii($0.19{;}{mu}m$), Dalvergia latifolia($0.20{;}{mu}m$) and Diospysos spp.($0.20{;}{mu}m$), Cercidiphum japonicum($0.24{;}{mu}m$) as good species while there was insignificant differences between softwoods and hardwoods. Tectona grands, Prunus serrulata var. spontanea and Abies holophylla showed rough surface with $1.53~2.63{;}{mu}m$ of $R_a$ values. The four kinds of rough indices($R_a,{;}R_z,{;}R_{max}{;}and{;}R_q$) showed very low correlations with moisture contents with the correlation coefficients. The $R_a{;}and{;}R_{max}$ also showed slight relationship with hardness.