기관회원 [로그인]
소속기관에서 받은 아이디, 비밀번호를 입력해 주세요.
개인회원 [로그인]

비회원 구매시 입력하신 핸드폰번호를 입력해 주세요.
본인 인증 후 구매내역을 확인하실 수 있습니다.

회원가입
서지반출
Clinical performance and failures of zirconia-based fixed partial dentures: a review literature
[STEP1]서지반출 형식 선택
파일형식
@
서지도구
SNS
기타
[STEP2]서지반출 정보 선택
  • 제목
  • URL
돌아가기
확인
취소
  • Clinical performance and failures of zirconia-based fixed partial dentures: a review literature
  • Clinical performance and failures of zirconia-based fixed partial dentures: a review literature
저자명
Triwatana. Premwara,Nagaviroj. Noppavan,Tulapornchai. Chantana
간행물명
The journal of advanced prosthodontics
권/호정보
2012년|4권 2호|pp.76-83 (8 pages)
발행정보
대한치과보철학회
파일정보
정기간행물|ENG|
PDF텍스트
주제분야
기타
이 논문은 한국과학기술정보연구원과 논문 연계를 통해 무료로 제공되는 원문입니다.
서지반출

기타언어초록

PURPOSE. Zirconia has been used in clinical dentistry for approximately a decade, and there have been several reports regarding the clinical performance and survival rates of zirconia-based restorations. The aim of this article was to review the literatures published from 2000 to 2010 regarding the clinical performance and the causes of failure of zirconia fixed partial dentures (FPDs). MATERIALS AND METHODS. An electronic search of English peer-reviewed dental literatures was performed through PubMed to obtain all the clinical studies focused on the performance of the zirconia FPDs. The electronic search was supplemented by manual searching through the references of the selected articles for possible inclusion of some articles. Randomized controlled clinical trials, longitudinal prospective and retrospective cohort studies were the focuses of this review. Articles that did not focus on the restoration of teeth using zirconia-based restorations were excluded from this review. RESULTS. There have been three studies for the study of zirconia single crowns. The clinical outcome was satisfactory (acceptable) according to the CDA evaluation. There have been 14 studies for the study of zirconia FPDs. The survival rates of zirconia anterior and posterior FPDs ranged between 73.9% - 100% after 2 - 5 years. The causes of failure were veneer fracture, ceramic core fracture, abutment tooth fracture, secondary caries, and restoration dislodgment. CONCLUSION. The overall performance of zirconia FPDs was satisfactory according to either USPHS criteria or CDA evaluations. Fracture resistance of core and veneering ceramics, bonding between core and veneering materials, and marginal discrepancy of zirconia-based restorations were discussed as the causes of failure. Because of its repeated occurrence in many studies, future researches are essentially required to clarify this problem and to reduce the fracture incident.